bullseyeglass.com • View topic - Keeping Texture of Stringer 1mm in Deep Slump

Keeping Texture of Stringer 1mm in Deep Slump

For discussion of processes related to using Bullseye glass, including kilnforming and kilncasting, torchwork, blowing and stained glass.

Keeping Texture of Stringer 1mm in Deep Slump

Postby eckazmier » Thu Jun 18, 2015 6:43 pm

Hello everyone,

I am hoping to make a deeper cone bowl comprised of 1 mm stringer. I would like to keep the texture of the stringer. Can anyone provide some insights on the min heatwork necessary to make the piece? Also, if I damn the piece during the tack fuse, is it possible to keep the piece to 1 mm ish thickness?

Thanks everyone!!
eckazmier
 
Posts: 5
Joined: Thu Jun 11, 2015 10:33 am

Return to Technique

Who is online