bullseyeglass.com • View topic - Devit

Devit

For discussion of processes related to using Bullseye glass, including kilnforming and kilncasting, torchwork, blowing and stained glass.

Devit

Postby meera » Sat Dec 19, 2020 7:58 am

Hi
After years of working with glass I am having devit problems. Glass is placed on thin fire paper, dammed using dams with shelf primer. The primer has been dried to 600F. Weird tasing on the edges touching the primer. Could the primer be old? Would appreciate help.
Thanks
Meera
Attachments
All Photos - 1 of 1.jpg
All Photos - 1 of 1.jpg (100.25 KiB) Viewed 1817 times
meera
 
Posts: 1
Joined: Thu Nov 10, 2011 3:36 pm

Return to Technique

Who is online

Users browsing this forum: No registered users and 1 guest

cron