Spring Green Opalescent | Glass Gallery | Bullseye Glass Products
All Styles
Choose by Color Family

All

Spring Green Opalescent 000126

  • Sheet Glass

  • Rod

  • Frit

  • Stringer

Spring Green Opalescent Sheet Glass

bullseye spring green opalescent kiln glass 000126-0030-x-xxxx

icon_striker.gif Striker

 

Contains

Sulfur

May React With

Copper, Lead, Silver

Cold Characteristics

Color variations common from minty-pastel to vibrant yellow-green.

Working Notes

Lighter coloration matures and becomes consistent to target upon firing. A sulfur glass. May react with lead and copper glasses to create dark interface (lead sulfide, copper sulfide).

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

Spring Green Opalescent Rod

bullseye spring green opalescent rod 000126-0576-F-xxxx

icon_striker.gif Striker

 

Cold Characteristics

Slight variations from one production run to another.

Working Notes

Torch: Lighter color and greater opacity than in sheet glass form. Keep it a bright chartreuse by working with a neutral to oxidizing flame atmosphere. Can turn gray in reduction.

Kiln: Lighter color and greater opacity than in sheet glass form.

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

Spring Green Opalescent Frit

spring green opalescent frit 000126-0002-F-xxxx

icon_striker.gif Striker

 

Working Notes

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

Spring Green Opalescent Stringer

spring green opalescent stringer 000126-0272-x-xxxx

icon_striker.gif Striker

 

Working Notes

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.